SINANO OpenIR  > 纳米器件及相关材料研究部  > 刘建平团队  > 期刊论文
题名: Investigation of rapid degradation in GaN-based blue laser diodes
作者: Wen, Pengyan(温鹏雁); Zhang, Shuming(张书明); Li, Deyao(李德尧); Liu, Jianping(刘建平); Zhang, Liqun(张立群); Shi, Dong; Zhou, Kun(周堃); Tian, Aiqin(田爱琴); Feng, Shiwei; Yang, Hui
刊名: SUPERLATTICES AND MICROSTRUCTURES
发表日期: 2016
DOI: 10.1016/j.spmi.2016.05.008
卷: 99
收录类别: SCI ; EI
文章类型: 期刊论文
部门归属: 纳米器件及相关材料研究部
英文摘要: Investigation of the degradation modes in GaN-based blue laser diodes grown by metal organic chemical vapor deposition (MOCVD) is carried out. Early failure of the LDs happened at the initial stage of the aging. After analysis of the electrical and thermal characteristics, local degradation of the active region is observed. Further investigation on the microstructures of the local regions shows that the early failure of the LDs is due to the local structure damage with the formation of gallium metal. (C) 2016 Elsevier Ltd. All rights reserved.
语种: 英语
JCR小类分区: 三区
WOS记录号: WOS:000390630200012
Citation statistics:
内容类型: 期刊论文
URI标识: http://ir.sinano.ac.cn/handle/332007/4643
Appears in Collections:纳米器件及相关材料研究部_刘建平团队_期刊论文

Files in This Item:
File Name/ File Size Content Type Version Access License
Wen-2016-Investigation of rapid degradation in.pdf(1744KB)期刊论文作者接受稿限制开放View 联系获取全文

Recommended Citation:
Wen, Pengyan,Zhang, Shuming,Li, Deyao,et al. Investigation of rapid degradation in GaN-based blue laser diodes[J]. SUPERLATTICES AND MICROSTRUCTURES,2016,99.
Service
Recommend this item
Sava as my favorate item
Show this item's statistics
Export Endnote File
Google Scholar
Similar articles in Google Scholar
[Wen, Pengyan(温鹏雁)]'s Articles
[Zhang, Shuming(张书明)]'s Articles
[Li, Deyao(李德尧)]'s Articles
CSDL cross search
Similar articles in CSDL Cross Search
[Wen, Pengyan(温鹏雁)]‘s Articles
[Zhang, Shuming(张书明)]‘s Articles
[Li, Deyao(李德尧)]‘s Articles
Related Copyright Policies
Null
Social Bookmarking
Add to CiteULike Add to Connotea Add to Del.icio.us Add to Digg Add to Reddit
文件名: Wen-2016-Investigation of rapid degradation in.pdf
格式: Adobe PDF
所有评论 (0)
暂无评论
 
评注功能仅针对注册用户开放,请您登录
您对该条目有什么异议,请填写以下表单,管理员会尽快联系您。
内 容:
Email:  *
单位:
验证码:   刷新
您在IR的使用过程中有什么好的想法或者建议可以反馈给我们。
标 题:
 *
内 容:
Email:  *
验证码:   刷新

Items in IR are protected by copyright, with all rights reserved, unless otherwise indicated.

 

 

Valid XHTML 1.0!